AISI 1025 Carbon Steel Normalized
VerifiedmetalAISI 1025 is a plain carbon steel (0.22-0.28% C) normalized to provide uniform microstructure and improved machinability through stress relief heat treatment. This condition offers moderate strength with good ductility and toughness, suitable for structural components and tubing applications requiring consistent properties without high hardness.
aerospacestructural
Compliance & Regulations
?Conflict Free?RoHS?REACH?TSCA?Prop 65
Filter by
Form
Orientation
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Ultimate Bearing Strength(Fbru) | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · t=... in · e/D=2 | — | |
Compressive Modulus(Ec) | — | Pa | 22°C · Sheet/Strip/Plate | — | |
Compressive Yield Strength(Fcy)2 entries | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · L · t=... in | — | |
| ↳ | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · LT · t=... in | — | |
Poisson's Ratio(ν) | — | - | 22°C | — | |
Shear Modulus(G) | — | Pa | 22°C · Sheet/Strip/Plate | — | |
Ultimate Shear Strength(Fsu) | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · t=... in | — | |
Ultimate Tensile Strength(σUTS)2 entries | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · L · t=... in | — | |
| ↳ | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · LT · t=... in | — | |
Yield Strength (0.2% offset)(σy)2 entries | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · L · t=... in | — | |
| ↳ | — | Pa | 22°C · Tubing · Normalized · AMS 5075 OR AMS-T-5066a · LT · t=... in | — | |
Young's Modulus(E) | — | Pa | 22°C · Sheet/Strip/Plate | — |
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
CTE vs Temperature(α(T)) | Curve (11 pts) | 1/K | — | — |
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | — | kg/m³ | 22°C | — |
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
Regulatory Screening
Environmental
Quality & Standards
Industry-Specific
RoHS, REACH, and Prop 65 statuses are validated against official substance lists (ECHA SVHC Candidate List, OEHHA Prop 65, RoHS Annex II). Other regulations are estimated from composition and material classification. All screening is a starting point for due diligence — always verify with your supplier before making compliance decisions.