A357.0 is a cast aluminum-silicon alloy (Al-7Si-0.6Mg) designed for aerospace and high-performance applications requiring good castability and elevated temperature strength. The T6 temper (solution heat-treated and artificially aged) provides enhanced mechanical properties with improved strength retention at service temperatures up to approximately 150°C.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Compressive Modulus(Ec) | 72.39 | GPa | 22°C · Casting | ||
Poisson's Ratio(ν) | 0.3300 | - | 22°C | ||
Shear Modulus(G) | 26.89 | GPa | 22°C · Casting | ||
Young's Modulus(E) | 71.71 | GPa | 22°C · Casting |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 2.685 | kg/m³ | 22°C |