7075 Aluminum T7352 is a high-strength aluminum-zinc alloy (Al-Zn-Mg-Cu) in an overaged temper condition that provides improved stress-corrosion cracking (SCC) resistance compared to T6, with slight sacrifice in yield strength, suitable for critical aircraft structures and pressure vessels exposed to sustained tensile stresses in marine and aerospace environments.
Compliance & Regulations
9 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Compressive Modulus(Ec) | 10,500 | ksi | 22°C · Bar/Rod | ||
Compressive Tangent Modulus vs Stress(Etn(σ))3 entries | Curve (13 pts) | ksi | 21°C · L | ||
| ↳ | Curve (14 pts) | ksi | 21°C · LT | ||
| ↳ | Curve (15 pts) | ksi | 21°C · ST | ||
Poisson's Ratio(ν) | 0.3300 | - | 22°C | ||
Shear Modulus(G) | 3,900 | ksi | 22°C · Bar/Rod | ||
Stress–Strain Curve (buckling region, ≤ 2% strain)(σ–ε (low-strain)) | — | ksi | 6 entriesClick to expand | ||
Young's Modulus(E) | 10,300 | ksi | 22°C · Bar/Rod | ||
3 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
CTE vs Temperature(α(T)) | Curve (5 pts) | µin/in·°F | — | ||
Specific Heat vs Temperature(Cp(T)) | Curve (5 pts) | BTU/(lb·°F) | — | ||
Thermal Conductivity vs Temperature(k(T)) | Curve (4 pts) | BTU/(hr·ft·°F) | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1010 | lb/in³ | 22°C |