7050 aluminum is a high-strength Al-Zn-Mg-Cu alloy used in aerospace structures and airframes where exceptional damage tolerance and fracture toughness are required. The T7452 temper provides stress-relief through controlled heat treatment to minimize residual stresses from forging while maintaining high static strength (yield and ultimate tensile strengths in the 435–480 MPa range) and improved resistance to stress-corrosion cracking compared to peak-aged tempers.
Compliance & Regulations
24 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Ultimate Bearing Strength(Fbru) | 91.00 – 131 | ksi | 16 entriesClick to expand | ||
Bearing Yield Strength(Fbry) | 73.00 – 101 | ksi | 16 entriesClick to expand | ||
Compressive Modulus(Ec) | 10,600 | ksi | 22°C · Hand Forging | ||
Compressive Tangent Modulus vs Stress(Etn(σ)) | — | ksi | 5 entriesClick to expand | ||
Compressive Yield Strength(Fcy) | 54.00 – 64.00 | ksi | 23 entriesClick to expand | ||
Elongation at Break(εf) | 3.000 – 9.000 | - | 20 entriesClick to expand | ||
Poisson's Ratio(ν) | 0.3300 | - | 22°C | ||
Shear Modulus(G) | 3,900 | ksi | 22°C · Hand Forging | ||
Ultimate Shear Strength(Fsu) | 39.00 – 42.00 | ksi | 8 entriesClick to expand | ||
S–N Curve (Wöhler)(S–N) | — | ksi | 9 entriesClick to expand | ||
Stress–Strain Curve (buckling region, ≤ 2% strain)(σ–ε (low-strain)) | — | ksi | 10 entriesClick to expand | ||
Ultimate Tensile Strength(σUTS) | 64.00 – 72.00 | ksi | 23 entriesClick to expand | ||
Yield Strength (0.2% offset)(σy) | 50.00 – 63.00 | ksi | 23 entriesClick to expand | ||
Young's Modulus(E) | 10,200 | ksi | 22°C · Hand Forging | ||
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 0.1020 | lb/in³ | 22°C |