Verifiedmetal5456 Aluminum is a 5xxx-series (Al-Mg) alloy with magnesium as the primary alloying element, offering excellent seawater corrosion resistance and weldability for marine and offshore applications. The H111 temper (strain-hardened and stress-relieved) provides moderate strength suitable for extruded structural components requiring controlled work-hardening without full annealing, with typical yield strength around 180 MPa and elongation of 10-12%.
aerospacestructural
Compliance & Regulations
?Conflict Free?FDA?RoHS?REACH?TSCA?Prop 65
Filter by
Form
Orientation
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Compressive Modulus(Ec) | Curve (19 pts) | ksi | — | — | |
Compressive Tangent Modulus vs Stress(Etn(σ))2 entries | Curve (11 pts) | ksi | 21°C · L | — | |
| ↳ | Curve (13 pts) | ksi | 21°C · LT | — | |
Elongation at Break(εf) | — | - | 22°C · Bar/Extrusion/Rod · H111 · AMS-QQ-A-200/7 · L · t=≤5.000 in | — | |
Poisson's Ratio(ν) | — | - | 22°C | — | |
Shear Modulus(G) | — | ksi | 22°C · Sheet/Plate | — | |
Stress–Strain Curve (buckling region, ≤ 2% strain)(σ–ε (low-strain))4 entries | Curve (9 pts) | ksi | 21°C · L | — | |
| ↳ | Curve (9 pts) | ksi | 21°C · L | — | |
| ↳ | Curve (9 pts) | ksi | 21°C · LT | — | |
| ↳ | Curve (8 pts) | ksi | 21°C · LT | — | |
Ultimate Tensile Strength(σUTS) | — | ksi | 22°C · Bar/Extrusion/Rod · H111 · AMS-QQ-A-200/7 · L · t=≤5.000 in | — | |
Yield Strength (0.2% offset)(σy) | — | ksi | 22°C · Bar/Extrusion/Rod · H111 · AMS-QQ-A-200/7 · L · t=≤5.000 in | — | |
Young's Modulus(E) | — | ksi | 22°C · Sheet/Plate | — |
N entriesMultiple entries per property — large groups are collapsed; click a summary row to expand. Use filters above to narrow by form / heat treatment / basis.
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
CTE vs Temperature(α(T)) | Curve (17 pts) | µin/in·°F | — | — | |
Thermal Conductivity vs Temperature(k(T)) | Curve (20 pts) | BTU/(hr·ft·°F) | — | — |
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | — | lb/in³ | 22°C | — |
Rows with are inherited from the base material
Verified Unverified Low confidence (<80%) Link to source
Regulatory Screening
Environmental
Safety & Biocompatibility
Quality & Standards
RoHS, REACH, and Prop 65 statuses are validated against official substance lists (ECHA SVHC Candidate List, OEHHA Prop 65, RoHS Annex II). Other regulations are estimated from composition and material classification. All screening is a starting point for due diligence — always verify with your supplier before making compliance decisions.