304L stainless steel is a low-carbon austenitic stainless steel alloy (Fe-Cr-Ni base) in wrought form, designed to minimize chromium carbide precipitation and intergranular corrosion during welding and high-temperature service. It is widely used in chemical processing, food and beverage production, pharmaceutical equipment, and marine environments where corrosion resistance combined with weldability is critical; engineers select 304L over standard 304 grade specifically when welded assemblies must maintain corrosion immunity in aggressive media without post-weld heat treatment.
Compliance & Regulations
10 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Elongation at Break(εf) | 40.00 – 45.00 | % | 7 entriesClick to expand | ||
Fatigue Strength (10⁶ cycles)(σf)2 entries | 240.0 | MPa | 20°C · 10⁶ cycles · air | ||
| ↳ | 185.0 | MPa | 288°C · 10⁶ cycles · air | ||
Stress–Strain Curve(σ–ε) | — | Pa | 8 entriesClick to expand | ||
Ultimate Tensile Strength(σUTS) | 515.0 | MPa | minimum · Sheet/Plate · ASTM A240 | ||
Yield Strength (0.2% offset)(σy)4 entries | 220.0 | MPa | 20°C · minimum · cold rolled coil and sheet (C) · EN 10088-2 | ||
| ↳ | 200.0 | MPa | 20°C · minimum · hot rolled coil and sheet (H) · EN 10088-2 | ||
| ↳ | 200.0 | MPa | 20°C · minimum · quarto plate (P) · EN 10088-2 | ||
| ↳ | 205.0 | MPa | minimum · Sheet/Plate · ASTM A240 | ||
Yield Strength vs Temperature(σy(T)) | Curve (4 pts) | Pa | specimen ASTM A370 round, 0.350 in. diameter, longitudinal | ||
Young's Modulus(E) | 200.0 | GPa | 20°C · EN 10088-1 | ||
Young's Modulus vs Temperature(E(T)) | Curve (29 pts) | Pa | notes | ||
7 interactive curves for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
CTE vs Temperature(α(T)) | Curve (15 pts) | 1/K | notes | ||
Specific Heat vs Temperature(Cp(T))3 entries | Curve (15 pts) | J/(kg·K) | notes | ||
| ↳ | Curve (15 pts) | J/(kg·K) | notes | ||
| ↳ | Curve (30 pts) | J/(kg·K) | notes | ||
Thermal Conductivity(k) | 15.00 | W/(m·K) | 20°C · EN 10088-1 | ||
Thermal Conductivity vs Temperature(k(T))2 entries | Curve (15 pts) | W/(m·K) | notes | ||
| ↳ | Curve (30 pts) | W/(m·K) | notes | ||
Thermal Diffusivity(α) | Curve (15 pts) | W/(m·K) | notes | ||
Coefficient of Thermal Expansion(α (CTE)) | 0.0000160 | 1/K | EN 10088-1 |
1 interactive curve for this material
Stress-strain, S-N fatigue and environmental knockdown curves are free with an account.
Create free account| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 7.900 | g/cm³ | EN 10088-1 | ||
Density vs Temperature(ρ(T)) | Curve (15 pts) | kg/m³ | notes |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Electrical Resistivity(ρe) | 7.300e-7 | Ω·m | 20°C · EN 10088-1 |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data