ZrTi2 is an intermetallic compound in the zirconium-titanium system, representing a ordered binary phase combining two refractory metals. While primarily of research and materials science interest rather than widespread industrial production, zirconium-titanium intermetallics are investigated for high-temperature structural applications where the combination of zirconium's corrosion resistance and titanium's strength could offer advantages, though processing and brittleness challenges have limited commercial adoption compared to conventional titanium alloys or zirconium-based nuclear materials.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 85.40 | GPa | — | ||
Poisson's Ratio(ν) | 0.4800 | - | — | ||
Shear Modulus(G) | 4.620 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.306 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 5.075 | µB | — | ||
Seebeck Coefficient(S) | -4.820 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1749 | eV/atom | — | ||
Formation Energy(ΔHf) | 0.1749 | eV/atom | — |