ZrAs₂ is an intermetallic compound composed of zirconium and arsenic, belonging to the class of transition metal arsenides. This material is primarily of research interest rather than established in mainstream industrial production, and is studied for its potential in semiconductor and electronic device applications due to its crystalline structure and electronic properties. The compound represents part of a broader family of refractory intermetallics that may offer thermal stability and electrical characteristics suitable for specialized high-temperature or high-performance electronics, though commercial adoption remains limited pending further development and processing optimization.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 110.0 | GPa | — | ||
| ↳ | 110.5 | GPa | — | ||
Poisson's Ratio(ν) | 0.2400 | - | — | ||
Shear Modulus(G)2 entries | 70.62 | GPa | — | ||
| ↳ | 71.78 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 6.825 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -14.71 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.8583 | eV/atom | — |