TlBiPbS3 is a ternary chalcogenide ceramic compound combining thallium, bismuth, lead, and sulfur—a materials chemistry composition typically studied in the context of solid-state physics and thermoelectric research. This compound belongs to the broader family of sulfide ceramics and represents an experimental material of interest for specialized electronic and thermal applications where heavy-element semiconductors are explored for their unique band structure properties.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 44.90 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3300 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 20.96 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 7.292 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.2450 | eV | DFT · OptB88vdW | ||
| ↳ | 0.4900 | eV | DFT · TBmBJ | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 20.03 | - | DFT · OptB88vdW | ||
| ↳ | 12.76 | - | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 14.73 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.04620 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.5092 | eV/atom | DFT · OptB88vdW |