Te4Mo3WS4 is a complex mixed-metal chalcogenide compound containing tellurium, molybdenum, tungsten, and sulfur. This is an experimental or research-phase material rather than an established commercial alloy, likely investigated for its potential in energy conversion, catalysis, or semiconductor applications given its multi-transition-metal composition. The combination of refractory metals (Mo, W) with chalcogens (Te, S) suggests interest in high-temperature stability, electronic properties, or catalytic activity relevant to advanced materials research.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 29.91 | GPa | — | ||
Poisson's Ratio(ν) | 0.01000 | - | — | ||
Shear Modulus(G) | 20.53 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.249 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.06100 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr) | 17.57 | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij) | 0.09246 | C/m² | — | ||
Seebeck Coefficient(S) | -49.72 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1252 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.4937 | eV/atom | — |