TbAgTe2 is an intermetallic compound composed of terbium, silver, and tellurium, belonging to the family of rare-earth metal chalcogenides. This material is primarily of research interest in solid-state physics and materials science rather than established industrial production, with potential applications in thermoelectric devices and quantum materials exploration. The combination of a rare-earth element (terbium) with a noble metal (silver) and chalcogen (tellurium) suggests study as a candidate for next-generation thermoelectric or magnetotransport applications, though practical engineering deployment remains limited.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 44.27 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2900 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 23.18 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 7.303 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.8690 | eV | DFT · OptB88vdW | ||
| ↳ | 1.297 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr) | 20.65 | - | DFT · OptB88vdW | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 11.98 | - | DFT · OptB88vdW | ||
| ↳ | 9.286 | - | DFT · TBmBJ | ||
Electron Effective Mass(m*e) | 0.6667 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.5000 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij)2 entries | 0.2646 | C/m² | DFT · OptB88vdW | ||
| ↳ | 0.1912 | C/m² | DFT · PBE | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | DFT · PBE | ||
Thermoelectric Power Factor(PF)2 entries | 0.00136 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00208 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -175.6 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 212.1 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 33.38 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.9308 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data