Strontium telluride (SrTe) is an inorganic compound semiconductor belonging to the II-VI semiconductor family, characterized by a rock-salt crystal structure similar to other alkaline-earth chalcogenides. While primarily a research material rather than a high-volume industrial compound, SrTe is investigated for thermoelectric applications, infrared optics, and solid-state physics studies due to its wide bandgap and thermal properties; it represents a less-common alternative to more established II-VI semiconductors like CdTe or PbTe, with potential utility in niche applications requiring specific lattice parameters or thermal performance in moderate-temperature regimes.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 35.60 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2400 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 24.54 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 4.806 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)3 entries | 3.730 | eV | Measured | ||
| ↳ | 1.772 | eV | DFT · OptB88vdW | ||
| ↳ | 2.310 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 11.31 | - | DFT · OptB88vdW | ||
| ↳ | 12.40 | - | DFT · PBE | ||
| ↳ | 16.87 range 7.910–25.83median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 6.304 | - | DFT · OptB88vdW | ||
| ↳ | 5.857 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Electron Effective Mass(m*e) | 0.3100 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 0.6500 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij) | 0.000 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.00243 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00204 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -177.4 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 229.8 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 16.36 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.855 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data