SrScBe is a ternary ceramic compound combining strontium, scandium, and beryllium elements, representing a research-phase material within the family of lightweight ceramic composites. While not yet established in mainstream industrial production, this compound is of interest in materials research for applications requiring combinations of low density, structural stiffness, and thermal stability—properties that make ceramic composites attractive alternatives to metallic systems in demanding aerospace and defense contexts. The specific chemistry suggests potential as a precursor or constituent phase in advanced composite systems, though further development would be needed to establish manufacturing scalability and cost-effectiveness for production applications.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 37.92 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2300 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 25.93 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 3.138 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | DFT · OptB88vdW | ||
| ↳ | 0.000 | eV | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.3267 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | 0.2430 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data