ScBiO2 is a bismuth-based oxide ceramic compound containing scandium, belonging to the family of mixed rare-earth and bismuth oxides. This material is primarily investigated in research contexts for applications requiring high-density ceramics with specific mechanical and thermal properties, particularly in solid-state chemistry and materials science studies exploring novel oxide compositions. It represents an experimental compound rather than an established commercial material, with potential applications in specialized ceramic systems where the combined properties of scandium and bismuth oxides offer advantages over single-oxide alternatives.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 100.5 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3100 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 51.25 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 7.503 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | DFT · OptB88vdW | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.5332 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -2.135 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data