Sc2BeBi is an experimental ternary ceramic compound composed of scandium, beryllium, and bismuth. This material belongs to the rare-earth and refractory ceramic family and is primarily of research interest rather than established commercial use. The combination of these elements suggests potential applications in high-temperature ceramics or specialized functional ceramics, though practical deployment remains limited pending further characterization of thermal stability, mechanical properties, and manufacturing feasibility.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.905 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | DFT · OptB88vdW | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.5144 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | 0.08526 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data