SbIO is an antimony iodine oxide ceramic compound that combines ionic and covalent bonding characteristics typical of mixed-valence metal halide oxides. This material is primarily of research interest for optoelectronic and photocatalytic applications, where the bandgap and crystal structure of antimony-based ceramics enable light absorption and charge separation. SbIO represents the broader family of bismuth and antimony halide perovskites and related compounds being investigated as alternatives to lead-based semiconductors, with potential advantages in environmental stability and tunable electronic properties for next-generation photovoltaics, photodetectors, and catalytic systems.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 48.70 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2400 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 29.36 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.841 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.197 | eV | DFT · OptB88vdW | ||
| ↳ | 1.640 | eV | DFT · TBmBJ | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 10.20 | - | DFT · OptB88vdW | ||
| ↳ | 8.284 | - | DFT · TBmBJ | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 30.38 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.5488 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.4223 | eV/atom | DFT · OptB88vdW |