Nb₃TeI₇ is a layered metal-halide compound combining niobium, tellurium, and iodine—a family of materials primarily explored in condensed matter physics and materials research rather than established industrial production. This compound is of interest as a potential two-dimensional or quasi-2D material for nanoelectronics and quantum device applications, with research focus on its electronic, mechanical, and exfoliation properties for layered material engineering.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 12.28 | GPa | — | ||
| ↳ | 30.30 | GPa | — | ||
Exfoliation Energy(Eexf) | 97.28 | meV/atom | — | ||
Poisson's Ratio(ν) | 0.2500 | - | — | ||
Shear Modulus(G)2 entries | 8.404 | GPa | — | ||
| ↳ | 19.76 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 5.993 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.4530 | eV | — | ||
Dielectric Constant (Relative Permittivity)(εr) | 12.66 | - | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Piezoelectric Modulus(eij)2 entries | 0.2343 | C/m² | — | ||
| ↳ | 0.2530 | C/m² | — | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | — | ||
Seebeck Coefficient(S) | -246 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000400 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.5641 | eV/atom | — |