Nb2AsC is a ternary metal carbide compound belonging to the MAX phase family—materials that combine ceramic hardness with metallic electrical and thermal conductivity. This is primarily a research and development material rather than an established commercial product; it has been synthesized and characterized in materials science laboratories but sees limited to no widespread industrial adoption at this time. The MAX phase family is valued for high-temperature applications, machinability, and damage tolerance, making compounds like Nb2AsC of interest for aerospace, defense, and extreme environment engineering where conventional ceramics or metals alone are inadequate.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K)2 entries | 205.7 | GPa | — | ||
| ↳ | 204.0 | GPa | — | ||
Shear Modulus(G)2 entries | 118.8 | GPa | — | ||
| ↳ | 126.0 | GPa | — | ||
Young's Modulus(E) | 312.0 | GPa | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 7.700 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg) | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -3.667 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.6357 | eV/atom | — |