NaSrAs is an inorganic ceramic compound belonging to the ternary arsenide family, combining sodium, strontium, and arsenic elements in a crystalline structure. This is a research-stage material with limited industrial deployment; it is primarily investigated for its electronic and optical properties within the broader class of semiconductor ceramics and intermetallic compounds. The material's potential applications lie in specialized optoelectronic devices and solid-state physics research, where its unique crystal structure and intermediate mechanical properties may offer advantages in niche applications that conventional semiconductors cannot fulfill.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 15.57 range 12.28–18.86median of 2 measurements | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.2700 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 6.890 range 4.790–8.990median of 2 measurements | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 3.802 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.059 | eV | DFT · OptB88vdW | ||
| ↳ | 1.899 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 18.77 | - | DFT · OptB88vdW | ||
| ↳ | 19.25 | - | DFT · PBE | ||
| ↳ | 13.40 range 8.750–18.05median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 9.141 | - | DFT · OptB88vdW | ||
| ↳ | 6.952 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Electron Effective Mass(m*e) | 0.1633 | me | DFT · OptB88vdW · 27°C | ||
Hole Effective Mass(m*h) | 1.103 | me | DFT · OptB88vdW · 27°C | ||
Magnetic Moment(μB) | 0.000 | µB | DFT · OptB88vdW | ||
Piezoelectric Modulus(eij)2 entries | 0.1277 | C/m² | DFT · OptB88vdW | ||
| ↳ | 0.1491 | C/m² | DFT · PBE | ||
Piezoelectric Stress Tensor(eij) | Matrix (redacted) | C/m² | DFT · PBE | ||
Thermoelectric Power Factor(PF)2 entries | 0.000492 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00125 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -66.34 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 204.8 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 25.17 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -0.9731 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data