LuBPd3 is an intermetallic ceramic compound combining lutetium, boron, and palladium in a 1:1:3 stoichiometric ratio. This material represents an experimental research composition within the boride-based intermetallic family, with potential applications in high-temperature structural materials where extreme thermal stability and chemical resistance are required. The combination of a refractory rare-earth element (lutetium) with transition metals (palladium) and boron suggests exploration for demanding aerospace, catalytic, or specialized electronic applications where conventional ceramics reach performance limits.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 10.75 | kg/m³ | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 0.000 | eV | — | ||
| ↳ | 0.000 | eV | — | ||
Magnetic Moment(μB) | 0.000 | µB | — | ||
Seebeck Coefficient(S) | -8.400 | µV/K | — |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.1517 | eV/atom | — | ||
Formation Energy(ΔHf) | -0.6332 | eV/atom | — |