K4I2O is an iodide-based ceramic compound belonging to the mixed-metal oxide ceramic family. This material represents an experimental or specialized research composition; limited industrial deployment data suggests it may be explored for applications requiring specific ionic or optical properties inherent to iodide ceramics. Engineers considering this material should recognize it as a candidate for niche electrochemical, photonic, or high-temperature applications where iodide chemistry offers advantages over conventional oxide ceramics, though commercial availability and long-term performance data remain restricted to specialized suppliers and research institutions.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Bulk Modulus(K) | 17.50 | GPa | DFT · OptB88vdW | ||
Poisson's Ratio(ν) | 0.3000 | - | DFT · OptB88vdW | ||
Shear Modulus(G) | 9.580 | GPa | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 2.967 | kg/m³ | DFT · OptB88vdW |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Band Gap(Eg)2 entries | 1.386 | eV | DFT · OptB88vdW | ||
| ↳ | 2.774 | eV | DFT · TBmBJ | ||
Dielectric Constant (Relative Permittivity)(εr)3 entries | 6.956 | - | DFT · OptB88vdW | ||
| ↳ | 7.660 | - | DFT · PBE | ||
| ↳ | 5.147 range 3.058–7.236median of 2 measurements | - | DFT · PBEsol | ||
High-Frequency Dielectric Constant (ε∞)(ε∞)2 entries | 3.248 | - | DFT · OptB88vdW | ||
| ↳ | 2.606 | - | DFT · TBmBJ | ||
Electronic Dielectric Tensor(ε∞) | Matrix (redacted) | - | DFT · PBE | ||
Total Dielectric Tensor(ε) | Matrix (redacted) | - | DFT · PBE | ||
Piezoelectric Modulus(eij) | 0.000 | C/m² | DFT · OptB88vdW | ||
Thermoelectric Power Factor(PF)2 entries | 0.000634 | W/(m·K²) | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 0.00175 | W/(m·K²) | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Seebeck Coefficient(S)2 entries | -98.28 | μV/K | DFT · OptB88vdW · n-type · 1e20 cm⁻³ · 327°C | ||
| ↳ | 335.1 | μV/K | DFT · OptB88vdW · p-type · 1e20 cm⁻³ · 327°C | ||
Spectroscopic Limited Maximum Efficiency (SLME)(SLME) | 7.520 | % | DFT · TBmBJ |
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Energy Above Hull(ΔEhull) | 0.000 | eV/atom | DFT · OptB88vdW | ||
Formation Energy(ΔHf) | -1.482 | eV/atom | DFT · OptB88vdW |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data