304 stainless steel is an austenitic iron-based alloy containing 18–20% chromium and 8–10.5% nickel, representing the most widely used stainless steel grade in industrial applications. It offers excellent corrosion resistance across a broad range of chemical environments and is readily weldable and formable, making it the default choice for applications requiring durability without specialized high-temperature or high-strength demands. Engineers select 304 over ferritic alternatives when corrosion performance is critical, and over duplex or precipitation-hardening grades when cost, ease of fabrication, and reliable room-temperature toughness are prioritized.
Compliance & Regulations
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Ultimate Bearing Strength(Fbru) | 1.117 – 2.489 | GPa | 9 entriesClick to expand | ||
Bearing Yield Strength(Fbry) | 0.3792 – 1.717 | GPa | 9 entriesClick to expand | ||
Compressive Modulus(Ec) | 179.3 – 193.1 | GPa | 5 entriesClick to expand | ||
Compressive Yield Strength(Fcy) | 0.1586 – 1.131 | GPa | 18 entriesClick to expand | ||
Elongation at Break(εf)2 entries | 40.00 | % | 22°C · Sheet/Strip · Annealed · AMS 5513 · LT · t=≤0.187 in | ||
| ↳ | 25.00 | % | 22°C · Sheet/Strip · 1/4 Hard · AMS 5910 · LT · t=... in | ||
Poisson's Ratio(ν) | 0.2700 | - | 22°C | ||
Shear Modulus(G) | 72.39 – 77.22 | GPa | 5 entriesClick to expand | ||
Ultimate Shear Strength(Fsu) | 344.7 – 689.5 | MPa | 9 entriesClick to expand | ||
Ultimate Tensile Strength(σUTS) | 0.5033 – 1.282 | GPa | 18 entriesClick to expand | ||
Yield Strength (0.2% offset)(σy) | 0.1793 – 1.055 | GPa | 18 entriesClick to expand | ||
Young's Modulus(E) | 179.3 – 199.9 | GPa | 5 entriesClick to expand | ||
| Property | Value | Unit | Conditions | Source | |
|---|---|---|---|---|---|
Density(ρ) | 7.916 | g/cm³ | 22°C |
Reference data from cited sources. Not verified or certified by MatWorld Inc. Verify against the source before use in design. Terms: engineering data